ATASEC 2019 Conference

Evaluation and Analysis of Flexible Pavement Overlay Thickness Using Asphalt Modified SIR 20 on Dawuan - Cikampek Road Using AASHTO 1993 Method
Lentien Febrianty (a), Suherman (b), Retno Utami (c)

a) Department of Civil Engineering Bandung State Polytechnic, Indonesia
Jalan Gegerkalong Hilir, Bandung 40012, Indonesia
lentienfebrianty[at]gmail.com
b) Department of Civil Engineering Bandung State Polytechnic, Indonesia
Jalan Gegerkalong Hilir, Bandung 40012, Indonesia
sxs142[at]yahoo.co.uk
c) Department of Civil Engineering Bandung State Polytechnic, Indonesia
Jalan Gegerkalong Hilir, Bandung 40012, Indonesia
retnoutami[at]polban.ac.id


Abstract

Flexible pavement structural evaluation using AASHTO 1993 method carried out based on deflection values from the survey using the Falling Weight Deflectometer (FWD) which will be used to calculate the Effective Structural Number (SNeff), Structural Number in Future (SNf) and overlay thickness. Flexible pavement is susceptible to rutting damage and permanent deformation. To increase rutting damage and permanent deformation resistance, Asphalt Concrete Wearing Course (ACWC) was being modified by adding SIR 20 material. In determining overlay thickness using AASHTO 1993 method, one of the factors influencing the thickness was properties of ACWC material. In this paper, a case study is carried out on the Raya Dawuan – Cikampek Road. The result of this case study were ACWC-Modified overlay thickness was thinner than ACWC-Normal. ACWC Modified pavement overlay structure thickness obtained at 80 mm meanwhile in ACWC-Normal was 100 mm.

Keywords: Flexible Pavement, SIR 20, Overlay Thickness.